scratch test


Scratch Test is conducted on a plaster applied with Cement + M Sand (1:5) and cured for 28 days.

We have conducted scratch test on the wall with the customer to show that the wall is poor on scratch test.

Failure in scratch test affects compressive strength and bond strength. It is a simple test to conduct on your walls. If you try to drive nails in failed walls, the nails will not stand. Meaning the customers will complain when try to install photo frames, wall mounted TVs etc.

Use RenderCon and avoid issues with Scratch Failure on your walls.

application video

Use OPC / PPC Cement Only. Do Not use PSC Cement. 

hydrophobicity comparison

First Video (Left) – Conventional (Non-Hydrophobic Wall)

Next Video (Right) – Hydrophobic Wall plaster with RenderCon ‘5S’

conventional vs rendercon

One Side is conventional plastering cured for 14 days. It has cracked / has poor strength

Other side is with RenderCon 5S. It is very good. 